Wu, Y. (author), Li, X.W. (author), Song, G.M. (author), Wang, Y.M. (author), Narita, T. (author)
Oxidation behavior of the uncoated base, Ni–Al coated and Re–Cr-Ni plus Ni–Al coated single-crystal (SC) Ni-based TMS-82+ superalloy is studied under cyclic air at 900ºC for 200 h to assess the oxidation resistance. Regardless of the coating processing, Ni–Al coating is effective in improving the oxidation resistance due to the formation of a...