document
van der Hoeven, W. (author)
Residual strength tests were performed on ARALL panels consisting of ARALL3 (3/2) laminates with bonded-on doublers. In particular, the effect of the doubler geometry (shape and thickness) on the residual strength was investigated. Prior to residual strength testing all panels were fatigue loaded to create a realistic type of damage, i.e. cracks...
report 1992
document
Schijve, J. (author), Jacobs, F.A. (author)
Fatigue tests were carried out on Redux and FM 123/5 bonded specimens at various stress levels, temperatures (RT to 65 C) and low and high test frequencies. Observations were made on the type of failure (bond line failure or sheet failure) and the significance of the adhesive squeezeout for crack nucleation. An analysis of the data and a...
report 1984
document
van der Hoeven, W. (author)
The effects of strain rate and temperature on the fracture behaviour of three structural adhesives (Redux 775, Metlbond 328 and EC 2216) were investigated using Double Cantilever Beam specimens. The test results were presented as critical elastic energy release rate data (G) to investigate whether this parameter could be used to characterize me...
report 1983
document
Vlieger, H. (author)
This report presents results of residual strength calculations, carried out on cracked panel configurations of various designs and provided with bonded stiffeners. The calculations were carried out using the computer program BOND. The results of these calculations are compared with results of residual strength tests, performed on panels of...