Schijve, J. (author), Jacobs, F.A. (author), Tromp, P.J. (author)
Flight-simulation tests based on a standardized gust load spectrum were carried out in normal air, very dry air and salt water. Specimen thicknesses were t = 2 mm and t = 10 mm, mean stress in flight was 70 or 55 MN/m². In all cases a significant effect of the environment was found. Fatigue lives for t = 10 ram were much shorter than for t = 2...
report 1976
Source URL (retrieved on 2024-06-09 08:40): https://repository.tudelft.nl/islandora/search/%20?amp%3Bamp%3Bf%5B0%5D=mods_genre_s%3A%22working%5C%20paper%22&%3Bamp%3Bf%5B1%5D=mods_subject_topic_ss%3A%22urban%5C%20redevelopment%22&%3Bf%5B0%5D=mods_subject_topic_ss%3A%22diversen%22&collection=research&f%5B0%5D=mods_genre_s%3A%22report%22&f%5B1%5D=mods_name_personal_author_namePart_family_ss%3A%22Jacobs%22&f%5B2%5D=mods_subject_topic_ss%3A%22fractography%22