Influence of build angles on thin-wall geometry and surface texture in laser powder directed energy deposition

Journal Article (2023)
Author(s)

P.R. Gradl (NASA Marshall Space Flight Center)

A. Cervone (TU Delft - Aerospace Engineering)

Piero Colonna (TU Delft - Aerospace Engineering)

Research Group
Space Systems Egineering
DOI related publication
https://doi.org/10.1016/j.matdes.2023.112352 Final published version
More Info
expand_more
Publication Year
2023
Language
English
Related content
Research Group
Space Systems Egineering
Volume number
234
Article number
112352
Downloads counter
282
Collections
Institutional Repository
Reuse Rights

Other than for strictly personal use, it is not permitted to download, forward or distribute the text or part of it, without the consent of the author(s) and/or copyright holder(s), unless the work is under an open content license such as Creative Commons.

Abstract

Metal additive manufacturing (AM) is being used for mission-critical applications in both developmental and production components, driven by economic and technical benefits. Laser powder directed energy deposition (LP-DED) allows manufacturing of thin wall geometric features for various components at diameters larger than 2 m. The characterization of geometric capabilities and limitations is critical for establishing guidelines for end users of the technology. Within this study, several samples of enclosed vertical tracks were fabricated and characterized using LP-DED, with 1 mm-thick walls and varying inclination angles up to 45° using the NASA HR-1 alloy (Fe-Ni-Cr). The wall thickness, melt pool, and surface texture, inclusive of waviness and roughness, were evaluated and results presented. The experimental results indicate that the wall thickness increases exponentially above 30°. The surface texture was shown to be dependent on 1) excess powder adherence, 2) melt pool irregularities causing material droop, and 3) excess material. The experiment revealed that the mean roughness reduces with increasing wall angle for the downskin surface. The upskin roughness reaches a maximum peak at 20° and slowly reduces as powder adheres within the valleys. Both the downskin and upskin surface textures are dominated by irregular waviness generated by the melt pool.