Enhanced efficiency and durability of nickel sulfide catalyst integrated with reduced graphene oxide
Exploring hierarchically porous structures for methanol oxidation reaction
Mehdi Salmi (Hassan II University of Casablanca)
Nabil Khossossi (TU Delft - Team Poulumi Dey)
Yousra Boudad (Hassan II University of Casablanca)
Charafeddine Jama (Université de Lille)
Fouad Bentiss (Chouaïb Doukkali University, Université de Lille)
Zaina Zaroual (Hassan II University of Casablanca)
Sanae El Ghachtouli (Hassan II University of Casablanca)
More Info
expand_more
Other than for strictly personal use, it is not permitted to download, forward or distribute the text or part of it, without the consent of the author(s) and/or copyright holder(s), unless the work is under an open content license such as Creative Commons.
Abstract
The growing demand for sustainable energy solutions highlights the need for advancements in electrocatalysts for direct methanol fuel cells (DMFCs). This study introduces a novel approach to enhance the efficiency and durability of nickel sulfide (NiS) catalysts. We developed a hierarchically porous structure integrated with reduced graphene oxide (rGO) on a nickel foam substrate. Using a dynamic hydrogen bubble template (DHBT) technique, we created a porous nickel scaffold. We then electrodeposited graphene oxide and NiS onto this scaffold, resulting in a hybrid structure termed NiS-rGO-Ni/NF. Characterization through SEM, XRD, and XPS confirmed that the catalyst has a highly porous structure with uniformly distributed Ni3S2 and Ni3S4 phases. The NiS-rGO-Ni/NF catalyst showed significant improvements over conventional NiS/NF. It achieved a peak current density of 84.10 mA/cm2 in the presence of 0.1 M methanol, compared to 30.32 mA/cm2 with NiS/NF. This enhancement is due to the porous nickel layer created using DHBT and the integration of rGO. Additionally, the NiS-rGO-Ni/NF catalyst demonstrated superior reaction kinetics, evidenced by a decrease in the Tafel slope from 204 mV/dec to 122 mV/dec. It also exhibited a remarkable increase in the electrochemically active surface area, reaching 179 cm2 compared to 22 cm2 for NiS/NF. These improvements in surface area and kinetics contribute to its excellent stability, with the catalyst maintaining consistent performance over 20 h of continuous operation. These results underscore the effectiveness of the NiS-rGO-Ni/NF catalyst in methanol oxidation and its potential for more efficient and stable electrochemical applications.