't Hart, W.G.J. (author)
A microscopic study has been performed on carbon composite fracture surfaces, using the Scanning Electron Microscope (SEM). It appears that the SEM is a useful tool to examine the fracture surface characteristics of composite materials failing under different loading conditions.
report 1976