Investigation on hot cracking during laser welding by means of experimental and numerical methods

Journal Article (2018)
Author(s)

H Gao (TU Delft - (OLD) MSE-5)

Gautam Agarwal (TU Delft - (OLD) MSE-5)

A Amirthalingam (Indian Institute of Technology Madras)

MJM Hermans (TU Delft - (OLD) MSE-5)

I.M. Richardson (TU Delft - (OLD) MSE-5)

Research Group
(OLD) MSE-5
Copyright
© 2018 H. Gao, G. Agarwal, M. Amirthalingam, M.J.M. Hermans, I.M. Richardson
DOI related publication
https://doi.org/10.1007/s40194-017-0524-z
More Info
expand_more
Publication Year
2018
Language
English
Copyright
© 2018 H. Gao, G. Agarwal, M. Amirthalingam, M.J.M. Hermans, I.M. Richardson
Research Group
(OLD) MSE-5
Issue number
1
Volume number
62
Pages (from-to)
71-78
Reuse Rights

Other than for strictly personal use, it is not permitted to download, forward or distribute the text or part of it, without the consent of the author(s) and/or copyright holder(s), unless the work is under an open content license such as Creative Commons.

Abstract

Hot cracking during laser welding of Transformation Induce Plasticity (TRIP) steel at the edges of steel flanges can be a problem. In this study, modified hot cracking tests were performed by welding on a single-side clamped specimen at various distances from the free edge, while the heat input and external constraints remained constant. In situ temperature and strain measurements were carried out using pre-attached thermocouples and digital image correlation, respectively. A thermal-mechanical finite element (FE) model was constructed and validated with the temporal and spatial data measured. From the validated FE model, the temperature and strain evolution in the weld mushy zone were studied. A critical strain for the onset of hot cracking in the TRIP steel examined was found to be in the range of 3.2 to 3.6%. This threshold was further evaluated and experimentally confirmed by welding with different heat inputs.