On the mix-mode fracture of carbon fibre/epoxy composites interleaved with various thermoplastic veils

Journal Article (2022)
Author(s)

Dong Quan (TU Delft - Structural Integrity & Composites, Shandong University)

Dongsheng Yue (Shandong University)

Yannan Ma (Shandong University)

Guoqun Zhao (Shandong University)

R.C. Alderiesten (TU Delft - Structural Integrity & Composites)

Research Group
Structural Integrity & Composites
Copyright
© 2022 D. Quan, Dongsheng Yue, Yannan Ma, Guoqun Zhao, R.C. Alderliesten
DOI related publication
https://doi.org/10.1016/j.coco.2022.101230
More Info
expand_more
Publication Year
2022
Language
English
Copyright
© 2022 D. Quan, Dongsheng Yue, Yannan Ma, Guoqun Zhao, R.C. Alderliesten
Research Group
Structural Integrity & Composites
Bibliographical Note
Green Open Access added to TU Delft Institutional Repository ‘You share, we take care!’ – Taverne project https://www.openaccess.nl/en/you-share-we-take-care Otherwise as indicated in the copyright section: the publisher is the copyright holder of this work and the author uses the Dutch legislation to make this work public. @en
Volume number
33
Reuse Rights

Other than for strictly personal use, it is not permitted to download, forward or distribute the text or part of it, without the consent of the author(s) and/or copyright holder(s), unless the work is under an open content license such as Creative Commons.

Abstract

This work studied the mix mode-I/II fracture behaviour of an aerospace-grade carbon fibre/epoxy composite that was interlayer-toughened by Polyamide-12 (PA), Polyphenylene-sulphide (PPS), Polyimide (PI), Polyethersulfone (PES) and Polyethylenimine (PEI) fibres. During the laminate curing process, the PA fibres melted, the PPS and PI fibres kept in their original form and the PES and PEI fibres dissolved in the epoxy matrix. This resulted in different toughening mechanisms of the veils for the mix mode-I/II fracture of the laminates, which was studied using a cracked lap-shear test. The main toughening mechanisms were observed to be plastic deformation and failure of the thermoplastic resin for the meltable PA veils, thermoplastic fibre debonding and bridging for the intact PPS and PI veils, and thermoplastic particle debonding and plastic void growth for the dissolvable PES and PEI veils. The experimental results revealed that the fibre debonding and bridging mechanism was superior for toughness enhancement, followed by the thermoplastic particle debonding and plastic void growth mechanism. For instance, interleaving the PPS and PEI veils increased the mix-mode fracture propagation energy of the laminates by 345% and 171%, respectively. However, the toughening performance of the PA and PI veils was poor, since the crack mainly propagated at the vicinity around the interlayer/laminate interface.