Failure and cracking of Inconel 718 air supply manifold support rods: A service-related contribution to lEPG TA 31
Damage assessment and preservation of an Egyptian silver vase (300 - 200 B.C.)
Influence of gust spectrum variations on fatigue crack growth behaviour of damage tolerant aluminium-lithium sheet materials
Fractographic and microstructural analysis of fatigue crack growth in Ti-6Al-4V fan disc forgings
Crack resistance, fracture toughness and instability in damage tolerant Al-Li alloys
Corrosion fatigue crack arrest in aluminium alloys
Microstructural and fractographic analysis of fatigue crack propagation in 2024-T351 and 2324-T39
Comparison of fracture toughness in titanium alloys IMI 550 and IMI 551
Evaluation of non-destructive inspection methods applied to milled step-down areas
Vacuum fatigue fracture in titanium alloy plate
Heat treatment studies of aluminium alloy type 7050 forgings. Interim report no. 3: Corroded-specimen fatigue tests and SCC propagation tests
Breukvlakonderzoek
Environmental effects on crack grwoth in flight-simulation tests on 2024-T3 and 7075-T6 material Supplement: Compilation of test data from an investigation on the effect of environment on crack growth under flight-simulation loading
Effects of crack plane orientation transitions on flight simulation fatigue crack propagation in a high strength aluminium alloy (7050)
Scanning electron microscopy of fracture surfaces of carton composite materials
Fractography of fatigue crack propagation in 2024-T3 nx 7075-T6 aluminium alloys tested in air and vacuum