Wanhill, R.J.H. (author), Leenheer, R. (author), Steijaert, J.P.H.M. (author), Koens, J.F.W. (author)
An Egyptian metal vase from the Ptolemaic period was investigated metallurgically and fractographically. The metal is nearly pure silver, and chemical analysis indicates it was obtained from the cupellation of lead. Despite its high purity (in archaeological terms) the metal is severely cracked and embrittled, with fractures mainly along grain...
report 1995