Wanhill, R.J.H. (author)Fracture toughness tests on two high strength titanium alloys, IMI 550 and 551, showed that the higher strength alloy, IMI 551, had a much lower toughness. The alloys were very similar in microstructure and fracture mechanisms. A number of model formulations for predicting fracture toughness were compared with the experimental results. This...report 1978