Skip to main content
TudRepo
Research repository
Education Repository
Cultural Heritage
Announcing TU Delft Repository replacement
On
2 July 2024
TU Delft Repository will be replaced with a fresh user friendly design with monthly new feature releases.
About
·
How to search
·
How to upload
Include full text
Search results
Back
Searched for: collection%253Air
(1 - 1 of 1)
Document type
Date
List view
Grid view
Print
Email
export CSV
export Excel
Improvement of the Oxidation Resistance of the Single-Crystal Ni-Based TMS-82+ Superalloy by Ni–Al Coatings with/without the Diffusion Barrier