Gavel, D.J. (author), Adema, A.T. (author), van der Stel, Jan (author), Sietsma, J. (author), Boom, R. (author), Yang, Y. (author)
Effect of nut coke addition with ferrous burden (pellet and sinter mixture) is experimentally investigated under simulated blast furnace conditions. Nut coke mixing degree was varied (0, 20 and 40 wt-%) as a replacement of the regular coke. During smelting, the ferrous bed evolves through three distinct stages of shrinkage due to indirect...
journal article 2020
document
Gavel, D.J. (author), Song, Qingshi (author), Adema, A.T. (author), van der Stel, Jan (author), Sietsma, J. (author), Boom, R. (author), Yang, Y. (author)
In the blast furnace, nut coke is utilized in a mixture with the ferrous burden to improve the gas permeability. Although applied in a broad range (10–40 mm, 2–23 wt-%), limited information is available on changed burden behaviour in its presence. In the present study, the detailed characterization was performed on the iron ore pellets quenched...
journal article 2018
document
Song, Q. (author)
The blast furnace consumes a large amount of high quality metallurgy coke (size 35-80 mm) in addition to ore in the form of pellets and sinter. This coke is the coarse fraction, derived from the coke plant. The fine fraction (8 -35 mm), arise after sieving, named nut coke, can’t be directly used in blast furnace. The fraction of smaller than 8...
doctoral thesis 2013