Searched for: subject%3A%22Adhesive%255C%252Bbonding%22
(1 - 2 of 2)
document
van der Hoeven, W. (author)
Fatigue and residual strength tests were done on doubler specimens consisting of an ARALL3 (3/2) laminate with a bonded-on fingertip doubler. The primary objective was to determine the effect of fatigue crack length on the residual strenght and delamination onset stress for this type of specimen. The specimens were precracked to variable crack...
report 1994
document
van der Hoeven, W. (author)
Fatigue crack growth and residual strength tests were done on ARALL2 (2/1) laminates with bonded-on doublers. The main test variables were the shape of the doubler (square and fingertip) and the thickness of the doubler (0.5 and 0.8 mm). All coupons had a starter notch in the outer aluminium face sheet of the ARALL2 laminate at the edge of the...
report 1994