Electron-Irradiation-Induced Degradation of Transfer Characteristics in Super-Junction VDMOSFET

Journal Article (2022)
Author(s)

Jing Jiang (Fudan University)

Shaogang Wang (Southern University of Science and Technology , TU Delft - Bio-Electronics)

X. Liu (Southern University of Science and Technology , TU Delft - Interactive Intelligence)

Jianhui Liu (Sky Chip Interconnection Technology Co)

Jun Li (Sky Chip Interconnection Technology Co)

Dexiang Zhou (Sky Chip Interconnection Technology Co)

Guo Qi Zhang (TU Delft - Electronic Components, Technology and Materials)

H.Y. Ye (Southern University of Science and Technology , TU Delft - Electronic Components, Technology and Materials, Chongqing University)

Chunjian Tan (TU Delft - Electronic Components, Technology and Materials, Chongqing University)

Research Group
Bio-Electronics
Copyright
© 2022 Jing Jiang, S. Wang, X. Liu, Jianhui Liu, Jun Li, Dexiang Zhou, Kouchi Zhang, H. Ye, C. Tan
DOI related publication
https://doi.org/10.3390/ electronics11132076
More Info
expand_more
Publication Year
2022
Language
English
Copyright
© 2022 Jing Jiang, S. Wang, X. Liu, Jianhui Liu, Jun Li, Dexiang Zhou, Kouchi Zhang, H. Ye, C. Tan
Research Group
Bio-Electronics
Issue number
13
Volume number
11
Reuse Rights

Other than for strictly personal use, it is not permitted to download, forward or distribute the text or part of it, without the consent of the author(s) and/or copyright holder(s), unless the work is under an open content license such as Creative Commons.

Abstract

High electric-field stress is an effective solution to the recovery of irradiated devices. In this paper, the dependence of the recovery level on the magnitude of gate voltage and duration is investigated. Compared with the scheme of high gate-bias voltage with a short stress time, the transfer characteristics are significantly recovered by applying a low electric field with a long duration. When the electric field and stress time are up to a certain value, the threshold voltage almost approaches the limitation, which is less than that before irradiation. Meanwhile, the effect of temperature on the recovery of the irradiated devices is also demonstrated. The result indicates that a high temperature of 175 °C used for the irradiated devices’ annealing does not play a role in promoting the recovery of transfer characteristics. In addition, to obtain a deep-level understanding of threshold degradation, the first-principles calculations of three Si/SiO2 interfaces are performed. It is found that new electronic states can be clearly observed in the conduction bans and valence bands after the Si-H/-OH bonds are broken by electron irradiation. However, their distribution depends on the selection of the passivation scheme. Ultimately, it can be observed that the threshold voltage linearly decreases with the increase in interface charge density. These results can provide helpful guidance in the deep interpretation of threshold degradation and the recovery of the irradiated super-junction devices.